Die Casting Defects

When zinc die casting first became available, it quickly gained recognition as a lightweight and cost-effective alternative to other alloys such as tin and lead. Over the past century, zinc alloys have made steady progress. While zinc has always been acknowledged for its high strength, the introduction of the Zamak family, and now the revolutionary EZAC™ alloy, has further enhanced the suitability of hot chamber die casting zinc alloys for a wide range of applications. Prior to the introduction of EZAC™, zinc was often overlooked for applications requiring high tensile strength, especially high-temperature tensile strength. Additionally, most zinc alloys exhibited low creep resistance compared to other materials. These areas of improvement were the primary focus during the creation of EZAC™, resulting in a zinc alloy that surpasses previous limitations.

Heat check

Heat check is a localised cracking or surface damage that can occur on the die casting mould. It is caused by thermal stress and cycling, which can be exacerbated by factors such as inadequate cooling, excessive overspray, or thick mould sections.

Soldering

Soldering is the formation of a thin metal layer on the casting surface. It is caused by erosion or dissolution of the die material due to uneven cooling, localised high temperatures, or improper metal flow. Soldering can be prevented by improving cooling, optimising part design, and improving metal flow management.

Cracks

Cracks are fractures or separations that can occur in the die casting. They can be caused by stress concentration, rapid cooling, and uneven thermal gradients. Cracks can be minimised by evaluating casting geometry, adjusting process timing, and enhancing thermal management.

Dimensional concerns

Dimensional concerns involve deviations from desired dimensions and tolerances in the die-cast part. They can be caused by unrealistic print tolerances, variations in process parameters, and thermal expansion effects. Dimensional concerns can be minimised by optimising tolerances, controlling process parameters, and considering thermal effects.

Flash

Flash is the excessive material that escapes between mould halves, forming thin fins or flanges on the casting. It can be caused by insufficient machine tonnage, die wear or misalignment, and suboptimal process parameters. Flash can be prevented by ensuring adequate machine tonnage, conducting regular die maintenance, and optimising process parameters.

Shrink porosity

Shrink porosity is characterised by voids or cavities formed due to the shrinkage of molten metal during solidification. It can be caused by non-uniform wall thickness and abrupt section transitions in the part design. Shrink porosity can be minimised by optimising casting geometry and implementing effective thermal management.

Flow marks (cold flow, non-fill, etc.)

Flow marks manifest as visible lines or streaks on the casting surface due to the flow of molten metal during mould filling. They can be caused by flaws in part geometry and inadequate gating and runner design. Flow marks can be minimised by refining part geometry, utilising flow simulation software, and implementing real-time monitoring.

A comprehensive understanding of common die casting defects, their causative factors, and practical solutions is pivotal in engineering high-quality castings. By implementing the solutions discussed in this article, manufacturers can effectively address defects, enhance production efficiency, and deliver products that meet exacting quality standards.

Related Resources
A Beginner's Guide to Die Cast Design
Understand the basics of die cast design and how to improve part function, durability, and manufacturability with Dynacast.
Read the Article
Die Casting Design FAQ
Explore our die casting design FAQ to understand critical design considerations, materials, and the most common industry queries.
Read the Article
Reducing Manufacturing Lead Time
Learn how early collaboration can streamline your production and give you a competitive edge.